Konpoze ak Fòm Upper/Vemp
Soulye espò anwo twal mouch-tire / anwo twal trikote / anwo ki pa koud
Anlè soulye fanm / miray tib / anlè soulye kwi
Anwo soulye travay / anwo soulye plaj / anwo pantouf andedan kay la
| Atik | L033A | L039 | LN347S | L349B | LV375B | LV6176 | W102 | W501 |
| Materyèl | EVA | EVA | TPU | TPU | TPU | Biyo TPU | PES | PA |
| Baz | Pa disponib | Pa disponib | PE | Pa disponib | Papye pèl | Papye pèl | Pa disponib | Pa disponib |
| Pwen fizyon | 55-75℃ | 55-85 ℃ | 90-110 ℃ | 65-120 ℃ | 50-115 ℃ | 50-120 ℃ | 70-130 ℃ | 60-130 ℃ |
| SijereLyezon℃ | 120 ~ 140 ℃ | 140 ~ 160 ℃ | 130-150 ℃ | 140 ~ 150 ℃ | 140 ~ 160 ℃ | 140 ~ 160 ℃ | 140 ~ 160 ℃ | 140 ~ 160 ℃ |
| Materyèl laminasyon | Twal baton, kanva,mikwofib, kwi,Twal Oxford, tranch EVA | Kwi otantik, may, kwi, twal trikote | ||||||
| ※Remak: Epesè, viskozite, lajè, ka Customized; pwosesis rekòmande a debogaj selon ekipman diferan. | ||||||||